"Original" Truck Bed Liner Gallon

Herculiner Truck Bed Liner is the Original DIY roll-on bed product. It is a polyurethane texturized non skid rubber formula providing 100% protection from scratches, rust dents and more. Herculiner can be used on wide range of projects including; truck bed liners, trailer flooring, trim, undercoating, car paint, boats and more. It adheres to a wide variety of surfaces including concrete, plastic, rubber, metal, wood, and fiberglass. Herculiner sets in 1-4 hours and cures to a black color in 10-12 hours. The 1 Gallon Can can cover an entire 6ft truck bed.

$104.99
  • Covers an 6-foot truck bed
  • Gallon covers - 55-60 sq ft.
  • Tough, textured formula has been the industry leader for over 12 years
  • Gloss black finish gives it a "like new" finish that lasts
  • Flexible and repairable—while bonding to just about anything
  • Our solvent-based product when applied to a surface cures stronger versus a water-based product
  • Provides a durable skid-resistant protective coating when cured
  • Herculiner isn't just for truck beds! With 101 uses it can be applied to wood, metal concrete, aluminum, asphalt, rubber, fiberglass, and most plastics, including PVC

Product Videos

"Original" Truck Bed Liner Gallon Video
"Original" Truck Bed Liner Gallon

"Original" Truck Bed Liner Gallon


Herculiner can be painted though, it is best to use a polyurethane based paint to coat the surface with. Colored polyurethanes may be a little harder to find, but because they are like material and have the same pliability, you will get the longest lasting coverage with it. The usage of polyurethane paint is recommended because other types of paint will not have the same pliability and will be more apt to crack and peel off at a much quicker rate. You can use any other paint if you'd like, except for lacquer, but it may not hold up as long as the polyurethane.

If you can, the best time to apply the paint is within 24 hours of the Herculiner becoming dry to the touch. It will be in it's most receptive state for paint at that time. So after you apply the final coat of Herculiner, give it the recommended one to four hour time frame to set or wait until the surface isn't tacky anymore, then put the paint on. If you go a prolonged amount of time between applying the product and painting, we usually recommend lightly sanding and cleaning the surface of the Herculiner before applying.

What you don't want to do is mix anything into the Herculiner before applying it, even if it is a urethane product. There is a specific amount of plasticizer for curing that is in the product that will be affected if anything additional is added and there is the chance that the tint would not be compatible with the polyurethane we use in our product. Even mixing one Herculiner color with another can cause curing issues because certain colors use different types of polyurethane as well.

Yes, Herculiner can be applied to virtually any surface including wood, metal, concrete, asphalt, rubber, fiberglass, and most plastics, including PVC, and even painted or primed steel and aluminum.

  • One quart of Xylene, Acetone or MEK (solution to prep the surface of the bed before coating)
  • Rubber gloves
  • Stir stick (we recommend a drill with a paint mixing attachment)
  • Paint tray and some rags
  • Tape for masking off areas

Yes, Herculiner can be applied between 32° F and 95° F. However, the colder the temperature and the lower the humidity, the longer the curing process will take. Additionally, it MUST BE APPLIED IN A WELL-VENTILATED AREA.

Yes, Herculiner adheres to itself.

Always use two coats. The first coat will form a good base. Then allow one to four hours to dry and apply a second coat to completely seal and bring out the shine. When applying the second coat, it is recommended to spread in the opposite direction to ensure complete coverage. *Note:One (1) gallon covers 6' beds with 2 coats. An extra quart is needed for 8' beds.

Use Xylene immediately to remove the product from your hands. Then wash hands with soap and water.

Herculiner is a permanent application. However, if the product is still wet, it can be removed using Xylene.

HERCULINER BED LINER INSTALLATION PROCESS

In just 3 easy steps, Herculiner Roll-On Bed Liner will create a durable skid-resistant protective coating to virtually any surface or material. It's great for wood, metal, concrete, aluminum, asphalt, rubber, fiberglass, and most plastics, including PVC.

PREP

Clean heavy dirt and grime from surface and mask off all areas to be painted. Scuff all paint surfaces where Herculiner is to be applied, leaving no glossy areas. Wipe down the surface with Xylene (Xylol), Acetone or MEK solution, and a rag.

APPLY

Stir Herculiner thoroughly before using and while you are working. This helps keeps the rubber particles suspended and assures an even application. Apply a light first coat. This acts as a "primer" for your second coat.

DRY

After the first coat has been applied, allow Herculiner to set up (approximately 1–4 hours or when it is no longer tacky). After you apply the second coat, let it cure for 24 hours.

ENJOY

Herculiner dries to the touch in 2 hours and is fully cured in 24 hours. When cured, Herculiner provides a tough, durable skid-resistant protective coating that won't chip, flake, or peel and prevents rust.

Before application
PREP
APPLY
DRY
ENJOY

Customer Reviews